Carbon Carbon Composites:
Carbon/carbon composites are carbon matrix composites reinforced by carbon fibers and their fabrics. With low density (< 2.0g/cm3), high strength, high specific modulus, high thermal conductivity, low coefficient of expansion, good friction performance, good thermal shock resistance, high dimensional stability, is now in the application of more than 1650℃, the highest theoretical temperature up to 2600℃, so it is considered to be one of the most promising high temperature materials.
The Reinforced C/C Composite from Semicera represents the forefront of material technology, combining lightweight characteristics with exceptional strength and thermal stability. This innovative composite is engineered for high-performance applications in industries such as aerospace, automotive, and semiconductor manufacturing.
At Semicera, we utilize advanced carbon fiber reinforcement to enhance the structural integrity of our C/C composites, ensuring they can withstand extreme temperatures and mechanical stress. The result is a material that excels in applications requiring durability and reliability.
With its outstanding properties, the Reinforced C/C Composite is an ideal choice for critical components, offering superior performance without compromising weight. Trust Semicera to provide cutting-edge solutions that meet your demanding industrial requirements.
Technical Data of Carbon/Carbon Composite |
|
||
Index |
Unit |
Value |
|
Bulk density |
g/cm3 |
1.40~1.50 |
|
Carbon content |
% |
≥98.5~99.9 |
|
Ash |
PPM |
≤65 |
|
Thermal conductivity (1150℃) |
W/m.k |
10~30 |
|
Tensile strength |
Mpa |
90~130 |
|
Flexural Strength |
Mpa |
100~150 |
|
Compressive strength |
Mpa |
130~170 |
|
Shear strength |
Mpa |
50~60 |
|
Interlaminar Shear strength |
Mpa |
≥13 |
|
Electric resistivity |
Ω.mm2/m |
30~43 |
|
Coefficient of Thermal Expansion |
106/K |
0.3~1.2 |
|
Processing Temperature |
℃ |
≥2400℃ |
|
Military quality, full chemical vapor deposition furnace deposition, imported Toray carbon fiber T700 pre-woven 3D needle knitting |
|
||
It can be widely used in the high temperature environment of various structure, heater and vessel. Compared with the traditional engineering materials, carbon carbon composite has the following advantages:
1) High strength
2) High temperature up to 2000℃
3)Thermal shock resistance
4) Low coefficient of thermal expansion
5) Small thermal capacity
6) Excellent corrosion resistance and radiation resistance
Application:
1. Aerospace. Because of the composite material has good thermal stability, high specific strength and stiffness. It can be used for manufacturing of aircraft brakes, wing and fuselage, satellite antenna and a support structure, solar wing and shell, large carrier rocket shell, engine shell, etc..
2. The automobile industry.
3. The medical field.
4. Heat-insulation
5. Heating Unit
6. Ray-insulation